Nominal diameter | Electrical resistance, μΩ * m (no more) The electrode/Nipple |
Bending strength, MPa (max.) The electrode/Nipple |
Young's modulus, GPa (no more) The electrode/Nipple |
Volume density, g/cm3 (not less) The electrode/Nipple |
Thermal coefficient of linear expansion (100 - 600 °C), x 10-6/℃ (no more) The electrode/Nipple |
Ash content, % (max) |
---|---|---|---|---|---|---|
75-200 мм |
Electrical resistance, μΩ * m (no more) 7,0/6,8The electrode/Nipple: |
Bending strength, MPa (max.) 10,0/15,0The electrode/Nipple: |
Young's modulus, GPa (no more) 12,0/14,0The electrode/Nipple: |
Volume density, g/cm3 (not less) 1,60/1,72The electrode/Nipple: |
Thermal coefficient of linear expansion (100 - 600 °C), x 10-6/℃ (no more) 2,6/2,3The electrode/Nipple: |
Ash content, % (max): 0,3 |
250-400 мм |
Electrical resistance, μΩ * m (no more) 7,0/6,8The electrode/Nipple: |
Bending strength, MPa (max.) 9,0/15,0The electrode/Nipple: |
Young's modulus, GPa (no more) 12,0/14,0The electrode/Nipple: |
Volume density, g/cm3 (not less) 1,60/1,72The electrode/Nipple: |
Thermal coefficient of linear expansion (100 - 600 °C), x 10-6/℃ (no more) 2,6/2,3The electrode/Nipple: |
Ash content, % (max): 0,3 |
450-600 мм |
Electrical resistance, μΩ * m (no more) 7,0/6,8The electrode/Nipple: |
Bending strength, MPa (max.) 8,0/15,0The electrode/Nipple: |
Young's modulus, GPa (no more) 12,0/14,0The electrode/Nipple: |
Volume density, g/cm3 (not less) 1,60/1,72The electrode/Nipple: |
Thermal coefficient of linear expansion (100 - 600 °C), x 10-6/℃ (no more) 2,6/2,3The electrode/Nipple: |
Ash content, % (max): 0,3 |