Nominal diameter | Electrical resistance, μΩ * m (no more) The electrode/Nipple |
Bending strength, MPa (max.) The electrode/Nipple |
Young's modulus, GPa (no more) The electrode/Nipple |
Volume density, g/cm3 (not less) The electrode/Nipple |
Thermal coefficient of linear expansion (100 - 600 °C), x 10-6/℃ (no more) The electrode/Nipple |
Ash content, % (max) |
---|---|---|---|---|---|---|
300-400 мм |
Electrical resistance, μΩ * m (no more) 6,2/5,0The electrode/Nipple: |
Bending strength, MPa (max.) 10,5/20,0The electrode/Nipple: |
Young's modulus, GPa (no more) 14,0/20,0The electrode/Nipple: |
Volume density, g/cm3 (not less) 1,67/1,74The electrode/Nipple: |
Thermal coefficient of linear expansion (100 - 600 °C), x 10-6/℃ (no more) 1,5/1,4The electrode/Nipple: |
Ash content, % (max): 0,3 |
450-500 мм |
Electrical resistance, μΩ * m (no more) 6,3/5,0The electrode/Nipple: |
Bending strength, MPa (max.) 10,5/20,0The electrode/Nipple: |
Young's modulus, GPa (no more) 14,0/20,0The electrode/Nipple: |
Volume density, g/cm3 (not less) 1,75/1,5The electrode/Nipple: |
Thermal coefficient of linear expansion (100 - 600 °C), x 10-6/℃ (no more) 1,5/1,4The electrode/Nipple: |
Ash content, % (max): 0,3 |
550-600 мм |
Electrical resistance, μΩ * m (no more) 6,0/4,3The electrode/Nipple: |
Bending strength, MPa (max.) 11,0/22,0The electrode/Nipple: |
Young's modulus, GPa (no more) 14,0/22,0The electrode/Nipple: |
Volume density, g/cm3 (not less) 1,66/1,78The electrode/Nipple: |
Thermal coefficient of linear expansion (100 - 600 °C), x 10-6/℃ (no more) 1,4/1,2The electrode/Nipple: |
Ash content, % (max): 0,5 |
650-700 мм |
Electrical resistance, μΩ * m (no more) 5,8/4,3The electrode/Nipple: |
Bending strength, MPa (max.) 11,0/22,0The electrode/Nipple: |
Young's modulus, GPa (no more) 14,0/22,0The electrode/Nipple: |
Volume density, g/cm3 (not less) 1,68/1,78The electrode/Nipple: |
Thermal coefficient of linear expansion (100 - 600 °C), x 10-6/℃ (no more) 1,4/1,2The electrode/Nipple: |
Ash content, % (max): 0,5 |